Glovebox Welding Systems: Controlling Moisture in Hermetic Sealing Hermetic sealing protects sensitive microelectronic devices by enclosing them in an airtight metal or ceramic package. Even with a sound weld, moisture trapped inside can compromise device performance and reliability. The sealing process must therefore control both weld integrity and the internal gas composition of the hermetically sealed package. Complete glovebox welding systems integrate precision welding equipment with a controlled-atmosphere enclosure. Successful sealing depends on three interconnected factors: materials, equipment, and process. These include package design and plating, welding equipment, fixtures and settings, and maintaining a controlled dry atmospheric condition. Hermetically sealed microelectronic packages can be found in a range of industries including but not limited to – telecommunications, photonics, aerospace, and defense. What is a glovebox welding system? Simply defined, a glovebox is an enclosure that provides a controlled environment for manipulating parts and/or performing manufacturing processes without exposing them directly to ambient air. Depending on the configuration, a complete system might incorporate: Precision welding equipment (resistance or laser) Vacuum bakeout ovens and/or antechambers Moisture monitoring and process gas analyzers Manual or automated operation These elements allow the welding equipment, atmospheric controls, and component preparation processes to operate as a coordinated manufacturing solution. Why is moisture control important in hermetic sealing? Moisture inside a hermetically sealed electronic package can affect the performance and reliability of its internal components. Moisture-related failures include: Corrosion of internal components and die pads Fogging of optical components Electrical instability and shorts caused by dendritic growth Stiction in microelectromechanical devices (MEMS) Moisture-related problems increase scrap and slow production when caught during manufacturing. If they go undetected, they can cause device failures in service. Controlling moisture during the hermetic sealing process helps reduce both risks. Where does moisture inside a hermetically sealed package come from? Moisture can enter a device package through several sources at different times during the process. Before the welding process, moisture present in the ambient air could be captured during the welding process. After the weld, it may enter via an inadequate weld joint, glass-to-metal seal, or a window-to-metal interface. Moisture can also originate from plating materials, epoxies, adhesives, and internal device materials that release gases during processing. How does a glovebox welding system remove and control moisture? A complete glovebox welding system addresses moisture through enclosure atmosphere control, component preparation, and controlled transfer into the welding environment. Controlled-atmosphere enclosure The enclosure maintains a dry environment through gas purging, pressure regulation, and moisture monitoring. Purging introduces dry gas into the enclosure while displacing moisture-containing gas. The system’s pressure and moisture controls monitor the environment during operation. Typical gases used include nitrogen, argon, and clean dry air. Vacuum bakeout ovens Moisture may remain in incoming components even when the enclosure atmosphere is dry. Vacuum bakeout ovens expose components to heat and vacuum to remove moisture and outgas undissolved volatile materials before welding. A typical bakeout condition might be 80–150°C for 2–24 hours at vacuum levels of approximately 200 mtorr or lower. Bakeout conditions must be developed for the specific materials and components being processed. Vacuum-backfill antechambers Antechambers allow parts to enter and exit the glovebox without exposing the main enclosure to ambient air. Vacuum and backfill cycles remove moisture-containing air from the transfer chamber and door interlocks help prevent exposure of the controlled atmosphere during component transfer. Potential sources of moisture contamination during this process include insufficient vacuum pump-down, leaky doors, faulty vacuum pumps, and contaminated backfill gas. What welding technologies can be integrated into a glovebox? AMADA WELD TECH offers glovebox systems that incorporate resistance welding, projection welding, or laser welding. The technology selected depends on the package design, materials, sealing requirements and budget. Parallel gap seam welding – Parallel gap seam welding uses wheel electrodes to deliver multiple overlapping weld spots, creating a continuous weld between a metal lid and a metal tub package or ceramic package with a metal seal ring. Weld current, force, spot spacing, speed, and electrode tracking are some of the process parameters that affect this process. Projection resistance welding – Projection welders use opposing electrodes to join a metal cap to a metal header containing an electronic device. The process controls the force and directs the current across the electrodes through the cap and the header. Heat generated during the welding process is concentrated along the annular or ring projection creating a hermetic seal between the 2 mating parts. Important considerations include electrode and part design, clamping speed, force and energy. Laser welding – Laser welding is a non-contact process which uses a laser beam to fuse materials upon contact. Often equipped with vision-directed motion and advanced seam tracking, these systems are ideal for implantable medical devices and thermal-sensitive electronic packaging requiring low heat input. For optimal weld quality, precise part fit-up and robust fixturing are critical. How can manufacturers determine whether a device is hermetically sealed, or moisture is trapped inside a sealed package? Manufacturers use a combination of destructive and non-destructive testing (NDT) methods to verify hermeticity and identify trapped internal moisture or volatile contaminants. Determining Hermeticity (Non-destructive Leak Testing) MIL-STD-883 (Method 1014 for hermeticity Before moisture can get trapped, or to prove the package won’t leak over time, manufacturers test the integrity of the weld joint. Helium Fine Leak Testing: The package is either welded with 10-15% helium tracer gas or placed in a pressurized chamber filled with helium gas (called “bombing”). If there is a microscopic leak, helium is forced inside the package. The device is then moved to a helium mass spectrometer vacuum chamber, which detects any helium leaking back out. PASS/ FAIL leak rates are specified in MIL-STD 883 (Method 1014). Gross Leak Testing (Bubble Test): To find larger leaks that helium might escape from too quickly, the device is submerged in a hot, inert fluorocarbon liquid. If a leak exists, the internal gas expands from the heat and creates a visible stream of bubbles. Optical Leak Test (OLT): A non-destructive method where the package is placed in a pressurized chamber under a laser interferometer. The laser measures the nanometer-scale deflection of the metal lid. If the lid stays bowed under pressure, the package is perfectly sealed; if the lid deforms and recovers, gas is leaking. Detecting Trapped Moisture and Undissolved Volatile Materials in a sealed device (Destructive Gas Analysis Testing) To see what is trapped inside a hermetically sealed package by sampling a batch, manufacturers use these specific tests: Internal Vapor Analysis (IVA) also known as Residual Gas Analysis (RGA): This is the industry standard (MIL-STD-883, Method 1018) for identifying trapped moisture, outgassing of undissolved volatile materials, intrusion of fluorocarbons during gross leak testing, hydrogen and oxygen. The package is placed in a vacuum chamber, punctured with a tiny needle, and the internal gas is drawn and analyzed using a mass spectrometer. It precisely measures the percentages of moisture, nitrogen, oxygen, and any outgassed volatile organic compounds (VOCs). PASS/ FAIL are specified in MIL-STD 883 (Method 1018. What should manufacturers investigate when a package fails moisture testing? There are multiple potential causes of RGA failures, including problems with the glovebox, component preparation, materials, and the welding process. For example, moisture contamination associated with the enclosure may require checking the moisture monitor, verifying the enclosure’s moisture level, leak testing the enclosure, and evaluating whether component transfers affect atmospheric conditions. When outgassing from internal materials is suspected, evaluate bakeout temperature and time, measuring the actual temperature at the components, and use process development experiments to optimize the bakeout schedule. Another option is to take a troubleshooting approach in which an empty package is vacuum baked, sealed in a controlled dry environment, and submitted for RGA testing to help distinguish enclosure-related contamination or from outgassing contaminants associated with internal device materials. How do you configure a complete glovebox welding system? AMADA WELD TECH’s web-based interactive glovebox configurator works as a learning tool and helps engineers navigate to various glovebox configurations offered by AMADA WELD TECH ranging from compact, low-cost entry-level enclosures to advanced systems with integrated welding equipment, automatic part handlers, gas analysis, and vacuum-bakeout capabilities. System selection depends on the required welding process, package design, atmosphere, and production requirements. MX2000 Modular Glovebox Welding System Explore AMADA WELD TECH glovebox systems and interactive glovebox configurator AX5000 Advanced Glovebox Welding System – Computerized atmospheric enclosure with integrated gas monitoring, independent vacuum pumping systems for ovens and antechambers, and a configurable modular design. MX2000 Glovebox Welding System – Modular glovebox configurable with ovens, antechambers, gas analyzers, moisture monitors, and environmental controls. Alpha Series Glovebox – Manually operated inert-atmosphere glovebox with vacuum bakeout, interchange, and gas control. Configurations are available for seam sealing and projection welding. Category: Hermetic Sealing, Gloveboxes Enjoyed this article? Share it!